19 Enovix Solved the Four Problems of Silicon Anodes 2. First Charge Efficiency Enovix Solution: "Pre-lithiation" process during manufacturing to insert additional lithium source to top off lithium trapped at formation into vertically short electrodes. 50mm Li source Impractical to diffuse lithium over the long 50mm dimension Vertical electrodes only 3mm high allow for fast diffusion of added lithium into silicon ENOVIX